WELDING INSPECTION CHECKLIST Created by ChecklistGuro (https://checklistguro.com) --- PRE-WELDING INSPECTION --- [ ] Joint Thickness (min/max) [ ] Root Gap (inches/mm) [ ] Bevel Angle (degrees) [ ] Joint Type (Butt, Fillet, Corner, Lap) [ ] Surface Conditions (Clean, Rust, Mill Scale, Paint, Contamination) [ ] Notes on Surface Conditions/Preparation [ ] Pre-Weld Photo(s) [ ] Date of Pre-Weld Inspection --- WELDER QUALIFICATION & DOCUMENTATION --- [ ] Welder ID Number [ ] Welding Process Qualification (SMAW (Stick), GMAW (MIG), GTAW (TIG), FCAW (Flux-Cored), Other (Specify in Long Text)) [ ] If 'Other' Process Selected, Specify: [ ] Qualification Expiration Date [ ] Welder Qualification Certificate (PDF/Image) [ ] Current Status (Active, Inactive, Suspended) [ ] Hours Welded for Qualification --- MATERIAL VERIFICATION --- [ ] Material Thickness (inches/mm) [ ] Material Grade (A36, A572 Grade 50, ASTM 1018, Other (Specify)) [ ] Material Specification (e.g., ASTM A36) [ ] Material Traceability Information (Heat Number, etc.) [ ] Material Coating (if applicable) (None, Galvanized, Painted, Other (Specify)) [ ] Coating Type (if applicable) --- JOINT PREPARATION --- [ ] Root Gap (mm) [ ] Bevel Angle (degrees) [ ] Surface Cleanliness Rating (1-5, 1=Poor, 5=Excellent) [ ] Cleaning Method Used (Grinding, Wire Brushing, Sandblasting, Mechanical Cleaning, Chemical Cleaning) [ ] Notes on Joint Condition/Preparation [ ] Joint Preparation Photos (Pre-Weld) [ ] Joint Type (Butt, Lap, T-Joint, Corner Joint) --- WELDING PROCEDURE SPECIFICATION (WPS) COMPLIANCE --- [ ] WPS Number Verified? (Yes, No, N/A) [ ] Welding Process (e.g., SMAW, GMAW, GTAW) (SMAW, GMAW, GTAW, Other) [ ] Preheat Temperature (°C) [ ] Interpass Temperature (°C) [ ] Welding Current (Amps) [ ] Shielding Gas Type (If applicable) (Argon, CO2, Argon/CO2 Mix, Other, Not Applicable) [ ] Notes on WPS Compliance Observations --- VISUAL WELD INSPECTION (DURING & AFTER) --- [ ] Weld Bead Width (mm) [ ] Weld Bead Height (mm) [ ] Undercut Depth (mm) [ ] Overlap (mm) [ ] Weld Profile (Cross-Section) (Convex, Concave, Flat, Other - Specify Below) [ ] Describe Other Weld Profile (if selected) [ ] Presence of Slag Inclusions (Yes, No, Uncertain) [ ] Describe any Weld Defects Observed (e.g., porosity, cracks, etc.) [ ] Upload Weld Photographs (Front, Side, Cross-Section) [ ] Overall Weld Appearance (General Condition) --- NON-DESTRUCTIVE TESTING (NDT) --- [ ] NDT Method Performed (Visual Testing (VT), Radiographic Testing (RT), Ultrasonic Testing (UT), Magnetic Particle Testing (MT), Liquid Penetrant Testing (PT), Other (Specify)) [ ] Description of NDT Procedure Used [ ] NDT Results Report (e.g., RT film, UT data) [ ] UT Scan Angle (Degrees) [ ] RT Exposure Time (Seconds) [ ] Acceptance Criteria Used (ASME Section V, AWS D1.1, Project Specification, Other (Specify)) [ ] Details of any Indications Found (Size, Location, Type) [ ] Disposition of Indications (Acceptable, Repair, Reject) --- POST-WELD HEAT TREATMENT (PWHT) --- [ ] Maximum Heating Rate (°C/hr or °F/hr) [ ] Soaking Temperature (°C or °F) [ ] Soaking Time (Hours) [ ] Cooling Rate (°C/hr or °F/hr) [ ] Heating Method (Furnace, Induction, Flame, Other (Specify in LONG_TEXT)) [ ] Details of 'Other' Heating Method (if selected above) [ ] Start Date/Time of PWHT [ ] End Date/Time of PWHT [ ] Any deviations from the specified PWHT procedure? [ ] PWHT Inspector Signature --- DOCUMENTATION & RECORD KEEPING --- [ ] Welding Inspection Date [ ] Welding Completion Date [ ] WPS Number Used (WPS-001, WPS-002, WPS-003, Other (Specify in Long Text)) [ ] Notes/Comments on WPS Application (If 'Other' selected above) [ ] Welder Qualification Certificates [ ] WPS Document (Copy) [ ] Inspection Results Summary [ ] Inspector Signature [ ] Inspector Name (Printed) --- END OF TEMPLATE --- Transform this text into a digital, automated, and trackable mobile app! Visit: https://checklistguro.com/templates/construction/welding-inspection-checklist (Click "Install Template" to launch your digital inspection tool immediately)